Abstract:
Highlights of the Second International RILEM Symposium on Demolition and Reuse of Concrete and Masonry, held in Tokyo, Japan, in November 1988, are described. Eighty-three papers were presented at the symposium: 54 on demolition and 29 on reuse. Included in the program was a panel presentation and discussion of demolition techniques, an exhibition and demonstration of new demolition machines, and a visit to the demolition site of the Japan Power Demonstration Reactor at the Tokai Establishment of the Japan Atomic Energy Research Institute.