Title: Tests of Full-Scale Continuous Reinforced Concrete Flat Slabs

Author(s): Alaa G. Sherif and Walter H. Dilger

Publication: Structural Journal

Volume: 97

Issue: 3

Appears on pages(s): 455-467

Keywords: analysis; bending moments; flat concrete plates; flat concrete slabs; flexural behavior; shear strength; slab-column connections; test setup.

DOI: 10.14359/4640

Date: 5/1/2000

Abstract:
A new test setup is used to test two full-scale 5 m (16 ft-5 in.) con-tinuous reinforced concrete flat slabs. The first slab was tested three times to failure after it had been repaired twice. Shear failures occurred at the edge and interior column-slab connections. Some slab-column connections contained shear studs as shear reinforce-ment. In the present paper, the experimental program as well as the test results related to the analyses of flat slabs and shear strength of slab-column connections are presented and discussed. Based on the test results, the shear strength of slab-column connections in a real slab system with realistic boundary conditions is assessed. The results are compared with the latest provisions of ACI, and with a proposed shear strength equation. Regarding the analysis of flat slabs, the test results are compared with the moments predicted by the equivalent frame method (EFM) and a linear elastic finite element analysis (FEM).


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer