International Concrete Abstracts Portal

  


Title: 363R-10: Report on High-Strength Concrete

Author(s): ACI Committee 363

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 65

Keywords: concrete properties; economic considerations; high-strength concrete; material selection; mixture proportions; structural applications; structural design; quality control.

DOI:

Date: 3/1/2010

Abstract:
This report summarizes currently available information about high-strength concrete (HSC). Topics discussed include selection of materials, concrete mixture proportions, ordering, batching, mixing, transporting, placing, quality control, concrete properties, structural design, economic considerations, and applications.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer