Abstract:
Reinforced concrete two-way slabs have evolved in the past century from simple solid slabs supported on beams on all sides to a multitude of complex slab systems, including irregular geometries. The demand for longer spans, advancements in forming and placing systems and the requirement for architectural esthetics, resulted in the innovation of today’s diverse two-way slab systems. When deciding on a slab system for certain project, designers now have the advantage of choosing from a wide variety of economical systems to suite the project requirements. Extensive experimental and analytical studies performed in the past hundred years and field observations of existing slabs helped researchers and engineers understand the complex behavior of two-way slab systems. With the increased understanding of the behavior of slabs, methods of analysis; design provisions and Code requirements have improved with each code cycle. This paper discusses the evolution of the different two-way spanning slab structural systems and reviews the historical development of the code provisions




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer