Title: The New NY Bridge Construction

Author(s): Brian P. Cresenzi

Publication: Concrete International

Volume: 38

Issue: 9

Appears on pages(s): 29-34

Keywords: quality, oversight, placement, sample

DOI:

Date: 9/1/2016

Abstract:
The existing Tappan Zee Bridge across the Hudson River between Westchester and Rockland Counties in New York State is being replaced with the New NY Bridge. A central requirement of the project is to achieve a 100-year service life without major rehabilitation. Cast-in-place concrete is a major material in the new bridge and will be in severe exposure conditions. The article discusses concrete production and concrete quality organization, as well as oversight testing and evaluation.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer