Title: Study of the behaviour of steel fiber reinforced concrete in shell structures and its post-cracking behaviour

Author(s): Domingo Cabo, A; Serna Ros, P.; Lázaro Fernández, C.

Publication: ACHE

Volume: 55

Issue: 233

Appears on pages(s): 89 - 101

Keywords:

DOI:

Date: 1/5/2004

Abstract:
The present paper proposes a material model for the steel fiber reinforced concrete which can be used in the design of shell structures. This material models was implementd in a non-linear FEM software carrying out the necessary tests of laboratory for its calibration. The paper includes an example of a singular shell structure that has been constructed using this material.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »  



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.