International Concrete Abstracts Portal

  


Title: Prestressing looses due to creep and relaxation: Study of varying steel types

Author(s): Corres Peiretti, H.; Sánchez Gálvez, V.; Elices Calafat, M.

Publication: ACHE

Volume: 36

Issue: 155

Appears on pages(s): 83 -

Keywords:

DOI:

Date: 1/3/1985

Abstract: