Title: Punching Capacity of Spread Footings Using ACI 318-19 and the Strip Model

Author(s): Scott Alexander, Carlos Ospina, and Eva Lantsoght

Publication: Symposium Paper

Volume: 357

Issue:

Appears on pages(s): 19-40

Keywords: arched strut, spread footings, punching shear, reinforced concrete, Strip Model

DOI: 10.14359/51738756

Date: 4/1/2023

Abstract:
In design, the sectional depth of reinforced concrete spread footings is usually governed by design code provisions for punching shear, which are derived primarily from experiments on slab-column connections. Previous experiments have shown that the punching behavior of concentrically loaded spread footings differs from that of slab-column connections. This paper describes punching of a concentrically loaded spread footing by combining conventional strut and tie modeling with the concept of an arch strip, part of the Strip Model. By itself, the Strip Model describes the behavior of slab-column connections under a variety of loading conditions. For spread footings, Strip Model concepts need to be combined with conventional strut and tie modeling to adequately describe load transfer in a concentrically loaded spread footing. Two methods are explored, each producing closed-form expressions for the footing capacity that agree well with experimental results (112 tests from the literature). The analyses make it possible to estimate the fraction of footing load that is carried by conventional strut and tie behavior. The experimental results are also compared to punching shear capacities in accordance with ACI 318-19. The Strip Model produces results with roughly the same average test-to-predicted ratio (in the order of 1.3) as ACI 318-19 but with a lower coefficient of variation (10.3% compared to 15.8%). This work shows how a lower-bound plasticity-based model can be used for the practical case of determining the capacity of reinforced concrete spread footings failing in punching shear.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer