Title: 363R-92: Report on High-Strength Concrete (Reapproved 1997)

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 55

Keywords: high-strength concrete

DOI:

Date: 1/1/1992

Abstract:

Note: 363R-92 is available in PDF format only. However, a newer version of this document exists. This document was replaced by 363R-10.

Currently available information about high-strength concrete is summarized. Topics discussed include selection of materials, concrete mix proportioning, batching, mixing, transporting, placing, control procedures, concrete properties, structural design, economics, and applications. A bibliography is included.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer