Abstract:
Numerical investigations of the strength of L-shaped short concrete columns subjected to combined axial load and biaxial bending were undertaken for the purpose of providing design aids for the structural engineer. Three sample design charts are presented, from a group of 50 to be published in 1979. General principles for computing, mapping, and handling interaction failure surfaces for columns of all shapes are summarized.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer