Shear-Critical Cracking in Slender Reinforced Concrete Beams

International Concrete Abstracts Portal

  


Title: Shear-Critical Cracking in Slender Reinforced Concrete Beams

Author(s): Woo Kim and Richard N. White

Publication: Structural Journal

Volume: 96

Issue: 5

Appears on pages(s): 757-765

Keywords: beam (supports); bond; cracking (fracturing); failure; flexural strength; reinforced concrete; shear properties

DOI: 10.14359/729

Date: 9/1/1999

Abstract:
This paper describes an experimental investigation into the cause of critical-shear cracking in slender reinforced concrete beams, using 20 simply supported reinforced concrete beams loaded to failure. The basic approach used was that the test beams were specially designed and fabricated to artificially isolate or add the effect of a certain fac-tor on the critical-shear cracking process. Then these test results were compared with results from ordinary control beams, and the differ-ences were analyzed to deduce the major cause for the initiation and the propagation of flexural shear cracking. The results indicated that the initiation of flexural shear cracking was strongly associated with the bond between concrete and reinforcement. Also, it was found that the propagation of the critical shear crack depended exclusively on the intensity of horizontal cracking. Some results were incompatible with the concept of shear strength of critical sections that form the basis of current shear design provisions. A more rational hypothesis of bond-induced shear failure mechanism is derived based on these experi-mental results.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer