Title: Thermal and Shrinkage Stresses in Composite Beams

Author(s): William Zuk

Publication: Journal Proceedings

Volume: 58

Issue: 9

Appears on pages(s): 327-340

Keywords: none

DOI: 10.14359/7987

Date: 9/1/1961

Abstract:
Equations are developed for both longitudinal and transverse stresses in composite beams under various conditions of temperature and shrinkage. Equations for the interface shears and moments between the slab and the beam are also presented of such induced stresses. to show the The induced order of magnitude stresses and deflections in themselves often standard specifications. exceed the values permitted




  