International Concrete Abstracts Portal

  


Title: Prediction of Modulus of Rupture of Concrete

Author(s): Frederic Legeron and Patrick Paultre

Publication: Materials Journal

Volume: 97

Issue: 2

Appears on pages(s): 193-200

Keywords: compressive strength; cracking (fracturing); curing; flexural strength; serviceability.

DOI: 10.14359/823

Date: 3/1/2000

Abstract:
Tensile strength of concrete is an important parameter for determining deflection and minimum flexural reinforcement. Many design codes use the modulus of rupture as the cracking strength. Relations giving the modulus of rupture as a function of concrete compressive strength are based on tests on concrete with compressive strength lower than 40 MPa. This paper presents a statistical study on 395 data points from a large number of research programs with concrete compressive strength ranging from 20 to 130 MPa. It further reveals that the data is largely scattered and that minimum, mean, and maximum values for the modulus of rupture should be defined. New relations are proposed, giving the modulus of rupture as a function of ÷f¢cand f¢c2/3. The use of the new relations in design codes is illustrated.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer