Abstract:
This is a progress report of an investigation the structural consisting performance of a floor construction cast-in- l of precast reinforced concrete joists with ace concretes ab. lor precast 2 or 2 1/2 in. reinforced con-Variables studied include: welded joist reinforcement, effectiveness of diagonal as compared with vertical stirrups, t pe of aggregate, type of bond of slab to joist, an d performance of precast as compared with cast-in-place slab.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.