Title:
Colored Architectural Concrete
Author(s):
Charles M. Dabney
Publication:
Concrete International
Volume:
6
Issue:
1
Appears on pages(s):
32-36
Keywords:
admixtures; architectural concrete;
chemical finishes; colored concrete; colors (materials);
curing; finishes; quality control; sealers.
DOI:
Date:
1/1/1984
Abstract:
Some methods and recommendations for consideration and use of systems for achieving quality color architectural concrete are presented. Included are sec-tions on integral mix systems, colored cements, chemical stains, dry shake colors, curing and maintenance, and coatings and sealers.*