Title: Shoring, Reshoring, and Safety

Author(s): N. J. Gardner

Publication: Concrete International

Volume: 7

Issue: 4

Appears on pages(s): 28-34

Keywords: age-strength relation; concrete construc-tion; fiat concrete slabs; form removal; formwork (con-struction); loads (forces); multistory buildings; safety; shoring; structural analysis

DOI:

Date: 4/1/1985

Abstract:
During the construction process, loads applied to supporting floors are great and can significantly exceed the supporting structure’s design capacity. A method for calculating the loads imposed during construction is presented. Data enabling the available structural strength to be calculated are also presented.*




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer