Description

This Reference Specification for the Architect/Engineer can be applied to projects providing minimum requirements for construction of concrete parking lots and site paving by citing it in the Project Specification. A mandatory requirements checklist and an optional requirements checklist are provided to assist the Architect/Engineer in supplementing the provisions of this Specification as required or needed by designating or specifying individual project requirements. Included are requirements for submittals, testing and inspection, concrete materials, distributed steel, embedded steel at joints, jointing and sealant material, forms, subgrade preparation, subbase, placing, texturing, curing, jointing, tolerances, and opening to traffic. The materials, processes, quality control measures, and inspection described in this document should be tested, monitored, or performed as applicable only by individuals holding the appropriate ACI certification or equivalent.

Keywords:

construction; curing; inspection testing; jointing; pavements; site paving; texturing.

 

Document Details

Author: ACI Committee 330

Publication Year: 2024

Pages: 13

Categories: Codes

Formats: Printed Document or Protected PDF/Web View

Table of Contents

PART 1—GENERAL, p. 2

1.1—Scope, p. 2

1.2—Interpretation, p. 2

1.3—Definitions, p. 2

1.4—Referenced standards, p. 3

1.5—Submittals, p. 4

1.6—Delivery, storage, and handling, p. 4

1.7—Preconstruction conference, p. 4

1.8—Quality assurance, quality control, and testing, p. 5

1.9—Acceptance of Work, p. 5

PART 2—PRODUCTS, p. 6

2.1—Materials, p. 6

2.2—Accessories, p. 9

2.3—Off-site fabrication, p. 9

PART 3—EXECUTION, p. 9

3.1—Preparation, p. 9

3.2—Transportation, p. 10

3.3—Installation, p. 10

3.4—Repair of cracks, p. 10

NOTES TO SPECIFIER, p. 11

General notes, p. 11

FOREWORD TO CHECKLISTS, p. 11

Checklist references, p. 11

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).