Description
This Specification covers minimum requirements for installing epoxy grouting between foundations and equipment bases. Included are requirements for materials, placement, forming, testing, repair, and quality control. A mandatory requirements checklist and an optional requirements checklist are provided to assist the Architect/Engineer in supplementing the requirements of this Specification as required or needed by designating or specifying individual project requirements.
Keywords:
cement grout; cementitious grout; epoxy grout; equipment grout; foundations; grout.
Table of Contents
PART 1—GENERAL, p. 2
1.1—Scope, p. 2
1.2—Interpretation, p. 2
1.3—Definitions, p. 2
1.4—Referenced standards, p. 3
1.5—Submittals, p. 3
1.6—Delivery, storage, and handling, p. 3
1.7—Quality assurance and control, p. 3
1.8—Acceptance of Work, p. 3
PART 2—PRODUCTS, p. 4
2.1—Materials, p. 4
2.2—Accessories, p. 4
PART 3—EXECUTION, p. 4
3.1—Preparation, p. 4
3.2—Installation, p. 5
3.3—Testing and inspection, p. 6
3.4—Repair, p. 6
3.5—Cleaning, p. 6
3.6—Hot weather curing, p. 6
NOTES TO SPECIFIER, p. 6
General notes, p. 6
Forward to checklists, p. 6
Return/Exchange Policy
Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.
Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.
Subscriptions These items are not eligible for return.
Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).