Notes/Preview
**A newer version of this document exists**
NEW VERSION
Description
This TechNote provides an answer to the question, "When corroded reinforcing steel is encountered in a repair, should the bar be undercut? How far should the bar be exposed along its length?"
TechNotes are a committee document that are narrowly focused, single-topic guides, usually practice oriented, that present a specific direction on a particular issue. ACI committee documents (including TechNotes) are reviewed and approved by ACI's Technical Activities Committee.
Keywords: corrosion; reinforcing steel; repair; ring anode effect; surface preparation
Document Details
Author: ACI Committee 364
Publication Year: 2011
Pages: 3
ISBN:
Categories: Repair
Formats: PDF
This document is Historical
Table of Contents
Introduction
Answer
Discussion
Summary
References
ERRATA INFO
Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the
Errata page.
Return/Exchange Policy
Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.
Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.
Subscriptions These items are not eligible for return.
Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).