Sustainability is one of the salient requirements in modern society. Structures frequently deteriorate because of aggressive service environments; consequently, federal and state agencies expend significant endeavors to maintain the quality of the structures. Among many factors, durability plays a major role in accomplishing the concept of sustainability. Extensive research has been conducted to understand the deterioration mechanisms of concrete and to extend the longevity of concrete members. Over the past decades, the advancement of technologies has resulted in durable construction materials such as advanced composites. This Special Publication (SP) contains nine papers selected from two technical sessions held in the ACI Spring Convention at Detroit, MI, in March 2017. All manuscripts were reviewed by at least two experts in accordance with the ACI publication policy.

 

Document Details

Publication Year: 2019

Pages: 160

ISBN: 9781641950541

Categories: Durability

Formats: PDF

Table of Contents

SP-331-1:

Thermal Detection of Subsurface Delaminations in Reinforced Concrete

Bridge Decks Using Unmanned Aerial Vehicle 1-14

Authors: Tarek Omar and Moncef L. Nehdi

SP-331-2:

Bond Behavior of Concrete Strengthened with FRP Laminates and NSM

Bars Subjected to Accelerated Aging using Freeze-Thaw Cycles 5-33

Authors: Ian Shaw, Hang Zhao and Bassem Andrawes

SP-331-3:

Cyclic Loading Behavior of CFRP-Wrapped Non-Ductile Beam-Column Joints. 34-54

Authors: Ali S. H. Zerkane, Yasir M. Saeed, and Franz N. Rad

SP-331-4:

Implications of High Plasticity Soils in Bridge MSE Wall Embankments 55-68

Author: Mark E. Williams

SP-331-5:

Long-Term Durability of GFRP Internal Reinforcement in Concrete Structures 69-79

Authors: Omid Gooranorimi, Doug Gremel, John J. Myers, Antonio Nanni

SP-331-6:

Improving the Durability of Impact Damaged PC Bridge Girders Using

CFRP Rod Panel Retrofit 80-100

Authors: Abheetha Peiris and Issam Harik

SP-331-7:

Experimental Investigation of CFRP Prestressed Concrete Beams 101-121

Authors: Yasir M. Saeed and Franz N. Rad

SP-331-8:

Behavior of Full-Scale Damaged Beams Repaired Using a Steel Reinforced

Polymer (SRP) Technique 122-135

Authors: Hayder Alghazali, Zuhair Al-Jaberi, Zena Aljazaeri, John J. Myers

SP-331-9:

Durability Investigations into CFRP-confined Concrete in H2SO4 136-150

Authors: Yongcheng Ji and Yail J. Kim

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).