SP-286: A Fracture Approach for FRP-Concrete Structures

SP-286: A Fracture Approach for FRP-Concrete Structures

Price: $ 73.50 USD

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

Note: The individual papers are also available as .pdf downloads. Please click on the following link to view the papers available, or call 248.848.3800 to order.

PURCHASE INDIVIDUAL PAPERS

Editors: Maria Lopez and Christian Carloni

Sponsored by: ACI Committees 440 & 446

Description

This CD contains 10 papers sponsored by ACI committees 440 & 446. The papers provide information on recent developments on the use of the framework of fracture mechanics to evaluate the performance of reinforced concrete (RC) structures strengthened with FRP composites. The information provided is useful to researcher and practicing engineer by presenting experimental and analytical tools based on a fracture approach that can assess the shear and flexural capacity of strengthened RC members

 

Document Details

Author: ACI Committees 440 & 446

Publication Year: 2012

ISBN: 9780870317651

Categories: Fiber-Reinforced Concrete

Formats: PDF

Table of Contents

1. Prediction of FRP Debonding Using the Global-Energy-Balance Approach

Authors: Chris J. Burgoyne, Mithila Achintha, Garfield X. Guan

2. Fracture approaches to debonding in FRP systems for double sided flexural upgrade

Authors: Oded Rabinovitch

3. Fracture Characteristics of Notched Concrete Beams Shear-strengthened with CFRP Sheets Subjected to High Temperature

Authors: Yail J. Kim, Amer Hmidan, Kyoung-Kyu Choi, and Siamak Yazdani

4. Effect of the fracture energy of the FRP/concrete interfacial behavior on beams strengthened in shear with EB-FRP

Authors: Ahmed Godat, Omar Chaallal

5. Shear Behavior of RC Structural Members Strengthened with FRP Materials: A Three Dimensional Numerical Approach

Authors: Tommaso D’Antino, Carlo Pellegrino, Valentina Salomoni, Gianluca Mazzucco

6. Shear strength of FRP reinforced concrete beams without stirrups:

verification of fracture mechanics formulation

Authors: Fabio Matta, Paolo Mazzoleni, Emanuele Zappa, Michael A. Sutton, Mohamed ElBatanouny, Aaron K. Larosche, Paul H. Ziehl

7. Fracture Mechanics Approaches to Debonding Behavior of Reinforced Concrete Members with Externally-bonded Fiber Reinforced Polymer Laminates

Authors: Corey Grace, Yang Yang, and Lesley Sneed

8. SRG application for structural strengthening of RC beams

Authors: F. da Porto, E. Stievanin, E. Gabin, M.R. Valluzzi

9. Material Characterization of the Concrete-Epoxy Interface under FRP Uwraps

Authors: JaeHa Lee, Maria M. Lopez

10. Application of Fracture Mechanics to Debonding of FRP from RC Members

Authors: Christian Carloni, Kolluru V. Subramaniam

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).