This document is a guide for the design and construction of fixed reinforced and prestressed concrete structures for service in a marine environment. Only fixed structures that are founded on the seabed are covered. Contents include materials and durability; dead, deformation, live, environmental, and accidental loads; design and analysis; foundations; construction and installation; and inspection and repair. The two appendixes discuss environmental loads such as wave, wind, and ice loads in detail, and the design of offshore concrete structures for earthquake resistance.
The MCP Online contains all new committee standards and reports released throughout the year. The most recently added include
PRC-357-24: Design and Construction of Fixed Offshore Concrete Structures - Guide
PRC-334.3-24: Construction of Concrete Shells Using Inflatable Forms - Report
PRC-211.10-24: Assessing Combined Aggregate Gradings—Guide
PRC-213.2-24: Internal Curing Using Prewetted Fine Lightweight Aggregate—TechNote
PRC-213.1-24: Curing Efficiency of Internally Cured Concrete—TechNote