Title: SP-065: Performance of Concrete in Marine Environment

Author(s): Editor: V.M. Malhotra

Publication: Symposium Paper

Volume: 65

Issue:

Appears on pages(s): 622

Keywords:

DOI: 10.14359/14117

Date: 8/1/1980

Abstract:
SP65 The performance of concrete in a marine environment has assumed importance with the discovery of offshore gas and oil deposits. A collection of 33 papers from 12 countries, which opens with a review of durability of concrete in sea water. This is followed by a series of papers dealing with permeability and physio-chemical studies of cement pastes, mortars, and concretes exposed to sea water. Other papers describe the mechanisms of corrosion of reinforcing steel, case histories of performance of concrete in sea water, accelerated tests, and repair techniques. Research reports cover performance of lightweight concrete in sea water and use of corrosion inhibitors.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer