Title: SP-163: Third CANMET/ACI Intl Conf on Performance of Conc in Marine Environment

Author(s): Editor: V.M. Malhotra

Publication: Symposium Paper

Volume: 163

Issue:

Appears on pages(s): 519

Keywords:

DOI: 10.14359/14203

Date: 8/1/1996

Abstract:
SP-163 This specialized publication offers 24 papers presented at the Third CANMET/ACI International Conference held on August 4 -9, 1996 in New Brunswick, Canada on the subject of Performance of Concrete in Marine Environments.




  