Title: SP-332: Responsibility in Repair Construction

Author(s):

Publication: Symposium Paper

Volume: 332

Issue:

Appears on pages(s): 98

Keywords: SP332

DOI: 10.14359/51719142

Date: 8/8/2019

Abstract:
The responsibilities for parties involved in a repair project may be significantly different than those traditionally encountered in new concrete construction. The new ACI 562 Code Requirements for Assessment, Repair and Rehabilitation of Concrete Buildings and corresponding ACI 563 Specifications for Repair of Concrete in Buildings identify requirements for the Licensed Design Professional and the contractor’s Specialty Engineer during repair programs. Differing lines of authority in repair are presented through industry practice recommendations and case studies, along with identification of industry needs, informing parties engaged in concrete evaluation and repair projects.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer