SP-265: Thomas T.C. Hsu Symposium: Shear and Torsion in Concrete Structures Topic: Shear Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 10/2009 Regular Price: $ 89.50 USD Member Price: $ 54.00 USD Become a Member More Info »
SP-272: Antoine E. Naaman Symposium - Four Decades of Progress in Prestressed Concrete, FRC, and Thin Laminate Composite Topic: Fiber-Reinforced Concrete Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 10/2010 Regular Price: $ 86.50 USD Member Price: $ 55.00 USD Become a Member More Info »
SP-274: Fiber Reinforced Self-Consolidating Concrete: Research and Applications CD Topic: Fiber-Reinforced Concrete Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 10/2010 Regular Price: $ 67.50 USD Member Price: $ 41.00 USD Become a Member More Info »
SP-275: Fiber-Reinforced Polymer Reinforcement for Concrete Structures 10th International Symposium Topic: Fiber-Reinforced Concrete Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 3/2011 Regular Price: $ 121.50 USD Member Price: $ 74.00 USD Become a Member More Info »
SP-284: Andy Scanlon Symposium on Serviceability and Safety of Concrete Structures: From Research to Practice CD Topic: Deflections Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 3/2012 Regular Price: $ 87.50 USD Member Price: $ 53.00 USD Become a Member More Info »
SP-285: Concrete Construction and Structural Evaluation: A Symposium Honoring Dov Kaminetzky Topic: Repair Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 5/2012 Regular Price: $ 75.50 USD Member Price: $ 45.00 USD Become a Member More Info »
SP-291: Corrosion of Reinforcing Steel in Concrete - Future Direction: Proceedings-Hope & Schupack Corrosion Symposium Topic: Corrosion Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 2/2013 Regular Price: $ 74.50 USD Member Price: $ 44.00 USD Become a Member More Info »
SP-296: Symposium Honoring James O. Jirsa's Contributions in Structural Concrete: A Time to Reflect Topic: Design Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 3/2014 Regular Price: $ 80.50 USD Member Price: $ 48.00 USD Become a Member More Info »
SP-306: Analytical and Finite Element Concrete Material Models - Comparison of Blast Response Analysis of One Way Slabs Topic: Blast Resistance , Finite Element Analysis Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 3/2016 Regular Price: $ 81.50 USD Member Price: $ 49.00 USD Become a Member More Info »
SP-307: Shrinkage Compensating Concrete - Past, Present, and Future Topic: Shrinkage Compensating Concrete Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 3/2016 Regular Price: $ 74.50 USD Member Price: $ 45.00 USD Become a Member More Info »
SP-308: Chloride Thresholds and Limits for New Construction Topic: Corrosion Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 6/2016 Regular Price: $ 49.50 USD Member Price: $ 29.00 USD Become a Member More Info »
SP-310: Fibre-Reinforced Concrete: From Design to Structural Applications FRC 2014: ACI-fib International Workshop Topic: Fiber-Reinforced Concrete Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 3/2017 Regular Price: $ 69.50 USD Member Price: $ 39.00 USD Become a Member More Info »
SP-314 Eco-Efficient and Sustainable Concrete Incorporating Recycled Post-Consumer and Industrial Byproducts Topic: Recycling Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 3/2017 Regular Price: $ 69.50 USD Member Price: $ 39.00 USD Become a Member More Info »
SP-315 ACI/fib International Symposium on Punching Shear in Structural Concrete Slabs: Honoring Neil M. Hawkins Topic: Reinforcement , Slabs Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 9/2017 Price:$ 69.50 USD Become a Member More Info »
SP-319: Reduction of Crack Width with Fiber Topic: Cracking , Fiber-Reinforced Concrete Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 6/2017 Regular Price: $ 69.50 USD Member Price: $ 39.00 USD Become a Member More Info »