SP-097: Analysis and Design of High-Rise Concrete Buildings Topic: Design Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 2/1987 Regular Price: $ 69.50 USD Member Price: $ 39.00 USD Become a Member More Info »
SP-098: Computer Applications in Concrete Technology Topic: Concrete Technology Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 3/1987 Regular Price: $ 69.50 USD Member Price: $ 39.00 USD Become a Member More Info »
SP-099: Polymer Modified Concrete Topic: Polymer Concrete Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 5/1987 Regular Price: $ 44.50 USD Member Price: $ 20.00 USD Become a Member More Info »
SP-1(02): Concrete Primer Topic: Materials Format: Printed Document or PDF Unit: IN-LB: Inch-Pound Units Language: English Author: Bryant Mather and Celik Ozyildirim Published: 10/2002 Regular Price: $ 65.50 USD Member Price: $ 40.00 USD Become a Member More Info »
SP-100: Concrete Durability: Proceedings of Katharine and Bryant Mather International Symposium Topic: Durability Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 4/1987 Regular Price: $ 69.50 USD Member Price: $ 39.00 USD Become a Member More Info »
SP-101: Computer Use for Statistical Analysis of ConcreteTest Data Topic: Testing Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 9/1987 Regular Price: $ 58.50 USD Member Price: $ 38.50 USD Become a Member More Info »
SP-102: Corrosion, Concrete, & Chlorides Topic: Corrosion Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 9/1987 Regular Price: $ 74.25 USD Member Price: $ 48.50 USD Become a Member More Info »
SP-103: Anchorage to Concrete Topic: Anchors Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 9/1987 Regular Price: $ 23.25 USD Member Price: $ 15.50 USD Become a Member More Info »
SP-104: Lewis H. Tuthill International Symposium: Concrete and Concrete Construction Topic: Concrete Technology Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 10/1987 Regular Price: $ 30.50 USD Member Price: $ 14.00 USD Become a Member More Info »
SP-105: Fiber Reinforced Concrete: Properties/Application Topic: Fiber-Reinforced Concrete Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 12/1987 Regular Price: $ 69.50 USD Member Price: $ 39.00 USD Become a Member More Info »
SP-106: Computer Applications in Concrete Technology--SanAntonio 1987 Topic: Concrete Technology Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 6/1988 Regular Price: $ 80.50 USD Member Price: $ 26.00 USD Become a Member More Info »
SP-107: Forming Economical Concrete Buildings -- Proceedings of the Third International Conference Topic: Formwork Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI, ASCE & TMS Published: 6/1988 Regular Price: $ 88.50 USD Member Price: $ 40.00 USD Become a Member More Info »
SP-108: Permeability of Concrete Topic: Permeability Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 8/1988 Regular Price: $ 38.75 USD Member Price: $ 28.50 USD Become a Member More Info »
SP-109: Concrete in Marine Environment Topic: Marine Concrete Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee E701 Published: 8/1988 Regular Price: $ 62.25 USD Member Price: $ 41.25 USD Become a Member More Info »
SP-110: Hyperbolic Paraboloid Shells Topic: Shells Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Published: 11/1988 Regular Price: $ 32.95 USD Member Price: $ 20.95 USD Become a Member More Info »