Cellular Concrete

Definition: a low-density product consisting of portland cement, cement-silica, cement-pozzolan, lime-pozzolan, or lime-silica pastes, or pastes containing blends of these ingredients and having a homogeneous void or cell structure, attained with gas-forming chemicals or foaming agents.- ACI Concrete Terminology


Cellular concrete is a mixture of cement, water, and preformed foam. The purpose of the foam is to supply a mechanism by which a relatively high proportion of stable air voids can be induced into the mixture and produce a cellular or porous solid upon curing of the mixture. When cellular concrete hardens, it has an oven-dry density of 50 lb/ft3 (.8 t/m3)or less.

Practice oriented papers and articles ON CELLULAR CONCRETE

Structural behavior of prestressed Ultra-High Performance Fibre-Reinforced Concrete beams with and without openings: comparison between experimental results and finite element modelling techniques

Publication: Special Publication
Date: 10/1/2020

Advances in X-Ray Computed Tomography for the Characterization of Cementitious Materials

Publication: Concrete International
Date: 9/1/2020

Development of Lightweight Roadside Safety Barriers using Foaming Admixture: Phase I - Properties of Flue Gas Desulfurization (FGD) Cellular Concrete

Publication: Special Publication
Date: 4/1/2007

Mechanical Properties of Plain AAC Material

Publication: Special Publication
Date: 3/1/2005

Structural Testing for Validating Reinforced AAC Design Provisions in the U.S.

Publication: Special Publication
Date: 3/1/2005

Technical Justification for Proposed Design Provisions for AAC Structures: Introduction and Shear Wall Tests

Publication: Special Publication
Date: 3/1/2005

Technical Justification for Proposed Design Provisions for AAC Structures: Assemblage Test and Development of R and CD Factors

Publication: Special Publication
Date: 3/1/2005

Acoustically Efficient Concretes Through Engineered Pore Structure

Publication: Special Publication
Date: 3/1/2005

Concrete Mixtures Made with Ternary Blended Cements Containing Fly Ash and Rice-Husk Ash

Publication: Special Publication
Date: 6/1/2001

Creep Effects During Launch of the Serio River Bridge (Title Change)

Publication: Concrete International
Date: 3/1/2000

Search all Articles on cellular concrete »

Education Publications on CELLULAR CONCRETE

There are no Education Publications on cellular concrete

View all ACI Education Publications on cellular concrete »

FREE ONLINE EDUCATION PRESENTATIONS ON cellular concrete (VIDEOS)

There are no Web Sessions on cellular concrete

View all free presentations on cellular concrete »


ACI Web Pages


Advanced Tips
Type Example Notes
Fuzzy kettle~ Contain terms that are close to the word kettle, such as cattle
Wild cat* Contain terms that begin with cat, such as category and the extact term cat itself
Exact-Single orange Contain the term orange
Exact-Phrase "dnn is awesome" Contain the exact phase dnn is awesome
OR orange bike Contain the term orange or bike, or both. OR, if used, must be in uppercase
orange OR bike
AND orange AND bike Contain both orange and bike. AND must be in uppercase
Combo (agile OR extreme) AND methodology Contain methodology and must also contain agile and/or extreme
Results Per Page:
select
Limit the search results with the specified tags
Limit the search results modified within the specified time
select
Limit the search results from the specified source
select
Search results must exactly contain the keywords

Please enter this 5 digit unlock code on the web page.