Definition: a siliceous or silico-aluminous material that will, in finely divided form and in the presence of moisture, chemically react with calcium hydroxide at ordinary temperatures to form compounds having cementitious properties (there are both natural and artificial pozzolans).- ACI Concrete Terminology
View all Documents on Pozzolan »
Publication: IJCSM Date: 11/30/2024
Publication: IJCSM Date: 9/30/2024
Publication: Materials Journal Date: 8/1/2024
Publication: Materials Journal Date: 5/1/2024
Publication: IJCSM Date: 1/31/2024
Publication: IJCSM Date: 11/30/2023
Publication: CRC Date: 8/1/2023
Publication: IJCSM Date: 7/31/2023
Search all Articles on Pozzolan »
Publication: Special Publication Date: 6/18/2024
Publication: Special Publication Date: 6/17/2024
Publication: Special Publication Date: 6/14/2024
Publication: Special Publication Date: 6/11/2024
Publication: Special Publication Date: 6/6/2024
Publication: Special Publication Date: 6/5/2024
There are no Certification Resources on Pozzolan
View all ACI Certification Resources on Pozzolan »
Cementitious Materials for Concrete
View all ACI Education Publications on Pozzolan »
On-Demand Course: Raw Natural Pozzolans in Concrete
On-Demand Course: Cementitious Materials for Concrete (Part 2)
On-Demand Course: Cementitious Materials for Concrete (Part 1)
On-Demand Course: Evaluation and Use of Harvested Fly Ash and Ground Bottom Ash as SCM in Concrete
On-Demand Course: The Role of Silica Fume in Reducing the Carbon Footprint of Concrete
On-Demand Course: Use of Bottom Ash as a Concrete SCM
On-Demand Course: The A to Zs of Supplementary Cementitious Material Reactivity
On-Demand Course: Improving Concrete Durability and Aesthetics with High Reactivity Metakaolin (HRM)
View all ACI Online Learning Courses on Pozzolan »
by Tarr
by Alastair Marsh
by Wang
by Isgor
by Cole Spencer
by Zunino
by R Doug Hooton
by Farshad Rajabipour
by Tokpatayeva
by Castillo
View all free presentations on Pozzolan »
Question: Definition of concrete, hydraulic cement, mortar, and grout
Question: Hardening of hydraulic cement
Question: The effect of entrained air on the workability of concrete
Question: Why is Type IV cement rarely produced and Type V cement rarely used?
Question: What is a pozzolan?
Question: What does a pozzolan do in the concrete?
Question: Using and handling pozzolans
Question: Pozzolans in mass concrete
Question: Importance of using pozzolans in hydraulic and environmental structures
Question: Are pozzolans all alike?
View all Frequently Asked Questions on Pozzolan»
October 26, 2025
Recent Advancements in Technologies for Utilizing Ground Glass Pozzolans (GGP) in Making Low Carbon Concrete
Reducing the Environmental Impact of Concrete through Innovative Materials
March 29, 2026
Lessons learned from field demonstration of natural pozzolans
Strategies for extending the service life of new and existing structures in a sustainable world
View all Pozzolan Events »
May 21, 2024
ACI Foundation Funds Eight New Research Projects
June 1, 2022
The Quest for Carbon-Neutral Concrete – Part 1
April 22, 2022
ACI Foundation Announces New Council Chairs
April 20, 2022
Charles K. Nmai Elected President of American Concrete Institute
April 7, 2020
ACI Foundation Councils Announce New Vice Chairs
April 2, 2019
Randall W. Poston Elected President of American Concrete Institute
January 30, 2019
ACI’s New Honorary Members
July 12, 2017
Leading by Example—ACI Research and Innovation
June 12, 2017
ACI Foundation Funds Four Research Projects for 2017
February 14, 2017
Recent Developments in Nanotechnology
View All ACI News »
Pozzolans
Calcined Clays Task Group
Search all Committees »
There are no Certifications on Pozzolan
View all certification programs »