Title:
If the Show Must Go On
Author(s):
Warren E. McPherson, Jr.
Publication:
Concrete International
Volume:
25
Issue:
11
Appears on pages(s):
48-50
Keywords:
DOI:
Date:
11/1/2003
Abstract:
This article is presented, not through the eyes of a scientist, but rather through those of a practitioner in the industry. Experts say that concrete strength must reach 500 psi (4 MPa) to resist one freezing and thawing cycle. I feel that the key is having the right circumstances, the right non-chloride accelerator, and above all, the right team.