Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
Staff Directory
ACI World Headquarters 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA Phone: 1.248.848.3800 Fax: 1.248.848.3701
ACI Middle East Regional Office Second Floor, Office #207 The Offices 2 Building, One Central Dubai World Trade Center Complex Dubai, UAE Phone: +971.4.516.3208 & 3209
ACI Resource Center Southern California Midwest Mid Atlantic
Feedback via Email Phone: 1.248.848.3800
ACI Global Home Middle East Region Portal Western Europe Region Portal
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: SP-039: Behavior of Concrete Under Temperature Extremes
Author(s): Editors: Carl Berwanger and V.M. Malhotra
Publication: Symposium Paper
Volume: 39
Issue:
Appears on pages(s): 216
Keywords:
DOI: 10.14359/14092
Date: 1/1/1973
Abstract: SP39 A discussion of Canadian research into effects of below normal and above normal temperatures on properties of concrete. The raction of temperature and age on thermal expansion and modulus of elasticity of concrete; vacuum processing; pulse velocity; field curing and protection are covered. Also included are effects of heat applied during curing and after placement, effects of steam injection and review of research by National Research Council of Canada on fire endurance of concrete masonry walls.