Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
Staff Directory
ACI World Headquarters 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA Phone: 1.248.848.3800 Fax: 1.248.848.3701
ACI Middle East Regional Office Second Floor, Office #207 The Offices 2 Building, One Central Dubai World Trade Center Complex Dubai, UAE Phone: +971.4.516.3208 & 3209
ACI Resource Center Southern California Midwest Mid Atlantic
Feedback via Email Phone: 1.248.848.3800
ACI Global Home Middle East Region Portal Western Europe Region Portal
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: SP-042: Shear in Reinforced Concrete--Volume 1 and 2
Author(s):
Publication: Symposium Paper
Volume: 42
Issue:
Appears on pages(s): 965
Keywords:
DOI: 10.14359/14095
Date: 1/1/1974
Abstract: SP42 Includes the latest data and concepts on shear strength. Contains 39 papers by authors from 10 countries covering the basic mechanics of shear transfer, and shear in medium-slender to slender beams. Also covered is shear in deep beams, brackets, walls, columns, and slabs. Descriptions of experimental and analytical studies of mechanisms by which shear is transferred in beams are presented.