Title: Selection/Design of Shotcrete for Temporary Support

Author(s): Ronald E. Heuer

Publication: Symposium Paper

Volume: 45

Issue:

Appears on pages(s): 160-174

Keywords:

DOI: 10.14359/17945

Date: 1/1/1974

Abstract:
[An outlined article] If shotcrete is being considered for use in support of an underground excavation, a problem of ground support has been encountered, or a potentional problem is anticipated. Identification of the problem is the first step in its solution. Most problems of ground support can be placed in one or more of four classes. . .