Description
This specification addresses bonding hardened concrete and steel to hardened concrete with an epoxy adhesive as defined for this purpose in ASTM C881. Included are controls for adhesive labeling, storage, handling, mixing and application, surface evaluation and preparation, as well as inspection and quality control.
The materials, processes, quality control measures, and inspections described in this document should be tested, monitored, or performed as applicable only by individuals holding the appropriate ACI certifications or equivalent.
Keywords: adhesive; bond; construction; epoxy; quality control; repair; safety; steel.
Document Details
Author: ACI Committee 548
Publication Year: 2013
Pages: 5
ISBN: 9780870318078
Categories: Polymer Concrete, Specifications
Formats: Protected PDF/Web View, ePub, or Kindle
This document is Withdrawn
Table of Contents
Part 1—General
1.1—Scope
1.2—Definitions
1.3—Referenced standards
1.4—Submittals
1.5—Product delivery, storage, and handling
1.6—Project conditions
Part 2—Products
2.1—Materials
Part 3—Execution
3.1—Preparation
3.2—Inspection and testing
3.3—Adhesive mixtures
3.4—Adhesive application
3.5—Cleanup
3.6—Safety
(nonmandatory portion follows)
Notes to specifier
General notes
Foreword to checklists
Mandatory requirements checklist
Optional requirements checklist
Submittals checklist
(mandatory portion follows)
Return/Exchange Policy
Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.
Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.
Subscriptions These items are not eligible for return.
Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).