Table of Contents
-LOW-STRENGTH CONCRETE AND CONTROLLED
LOW-STRENGTH MATERIAL (CLSM) PRODUCED WITH
CLASS F FLY ASH, by T.R. Naik and B.W. Ramme
-OPTIMIZATION OF FLOWABLE FILL MIX PROPORTIONS,
by M.E. Ayers, S.Z. Wong, and W. Zaman
-DURABILITY FACTORS AFFECTING CLSM, by W.E. Brewer
-FREEZING AND THAWING DURABILITY AND EARLY
SET AND STRENGTH DEVELOPMENT OF CLSM, by
T.E. Nantung and C.F. Scholer
-FLOWABLE BACKFILL FOR PIPELINE BEDDING AT
THE DENVER INTERNATIONAL AIRPORT, by D.A. Clem,
K.D. Hansen, and J.B. Kowalsky
-SOIL-CEMENT SLURRY PIPE EMBEDMENT, by A.K. Howard