Table of Contents
Page ASTM Standard Designation
1 A82/A82M-07 Standard Specification for Steel Wire, Plain, for Concrete Reinforcement
5 A184/A184M-06 Standard Specification for Welded Deformed Steel Bar Mats for Concrete Reinforcement
8 A185/A185M-07 Standard Specification for Steel Welded Wire Reinforcement, Plain, for Concrete
14 A242/A242M-04ε1 Standard Specification for High-Strength Low-Alloy Structural Steel
17 A307-07a Standard Specification for Carbon Steel Bolts and Studs, 60,000 psi Tensile Strength
22 A416/A416M-06 Standard Specification for Steel Strand, Uncoated Seven-Wire for Prestressed Concrete
27 A421/A421M-05 Standard Specification for Uncoated Stress-Relieved Steel Wire for Prestressed Concrete
31 A496/A496M-07 Standard Specification for Steel Wire, Deformed, for Concrete Reinforcement
37 A497/A497M-07 Standard Specification for Steel Welded Wire Reinforcement, Deformed, for Concrete
42 A500/A500M-07 Standard Specification for Cold-Formed Welded and Seamless Carbon Steel Structural Tubing in Rounds and Shapes
47 A501-07 Standard Specification for Hot-Formed Welded and Seamless Carbon Steel Structural Tubing
55 A572/A572M-07 Standard Specification for High-Strength Low-Alloy Columbium- Vanadium Structural Steel
59 A588/A588M-05 Standard Specification for High-Strength Low-Alloy Structural Steel, up to 50 ksi [345 MPa] Minimum Yield Point, with Atmospheric Corrosion Resistance
62 A615/A615M-07 Standard Specification for Deformed and Plain Carbon-Steel Bars for Concrete Reinforcement
68 A706/A706M-06a Standard Specification for Low-Alloy Steel Deformed and Plain Bars for Concrete Reinforcement
74 A722/A722M-07 Standard Specification for Uncoated High-Strength Steel Bars for Prestressing Concrete
79 A767/A767M-05 Standard Specification for Zinc-Coated (Galvanized) Steel Bars for Concrete Reinforcement
83 A775/A775M-07a Standard Specification for Epoxy-Coated Steel Reinforcing Bars
93 A820/A820M-06 Standard Specification for Steel Fibers for Fiber-Reinforced Concrete
97 A884/A884M-06 Standard Specification for Epoxy-Coated Steel Wire and Welded Wire Reinforcement
103 A934/A934M-07 Standard Specification for Epoxy-Coated Prefabricated Steel Reinforcing Bars
119 A955/A955M-07a Standard Specification for Deformed and Plain Stainless-Steel Bars for Concrete Reinforcement
130 A970/A970M-06 Standard Specification for Headed Steel Bars for Concrete Reinforcement
138 A992/A992M-06a Standard Specification for Structural Steel Shapes
141 A996/A996M-06a Standard Specification for Rail-Steel and Axle-Steel Deformed Bars for Concrete Reinforcement
146 A1022/A1022M-07 Standard Specification for Deformed and Plain Stainless Steel Wire and Welded Wire for Concrete Reinforcement
155 A1035/A1035M-07 Standard Specification for Deformed and Plain, Low-Carbon, Chromium, Steel Bars for Concrete Reinforcement
160 A1044/A1044M-05 Standard Specification for Steel Stud Assemblies for Shear Reinforcement of Concrete
165 C29/C29M-97(2003) Standard Test Method for Bulk Density (“Unit Weight”) and Voids in Aggregate
169 C31/C31M-06 Standard Practice for Making and Curing Concrete Test Specimens in the Field
175 C33-03 Standard Specification for Concrete Aggregates
186 C39/C39M-05ε1 Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens
193 C42/C42M-04 Standard Test Method for Obtaining and Testing Drilled Cores and Sawed Beams of Concrete
199 C94/C94M-06 Standard Specification for Ready-Mixed Concrete
210 C109/C109M-05 Standard Test Method for Compressive Strength of Hydraulic Cement Mortars (Using 2-in. or [50-mm] Cube Specimens)
219 C144-04 Standard Specification for Aggregate for Masonry Mortar
221 C150-05 Standard Specification for Portland Cement
229 C172-04 Standard Practice for Sampling Freshly Mixed Concrete
232 C192/C192M-06 Standard Practice for Making and Curing Concrete Test Specimens in the Laboratory
240 C231-04 Standard Test Method for Air Content of Freshly Mixed Concrete by the Pressure Method
249 C260-06 Standard Specification for Air-Entraining Admixtures for Concrete
252 C330-05 Standard Specification for Lightweight Aggregates for Structural Concrete
256 C494/C494M-05a Standard Specification for Chemical Admixtures for Concrete
266 C496/C496M-04 Standard Test Method for Splitting Tensile Strength of Cylindrical Concrete Specimens
271 C567-05a Standard Test Method for Determining Density of Structural Lightweight Concrete
274 C595-07 Standard Specification for Blended Hydraulic Cements
281 C618-05 Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete
284 C685/C685M-01 Standard Specification for Concrete Made by Volumetric Batching and Continuous Mixing
293 C845-04 Standard Specification for Expansive Hydraulic Cement
296 C989-06 Standard Specification for Ground Granulated Blast-Furnace Slag for Use in Concrete and Mortars
301 C1012-04 Standard Test Method for Length Change of Hydraulic-Cement Mortars Exposed to a Sulfate Solution
307 C1017/C1017M-03 Standard Specification for Chemical Admixtures for Use in Producing Flowing Concrete
316 C1116/C1116M-06 Standard Specification for Fiber-Reinforced Concrete
323 C1157-03 Standard Performance Specification for Hydraulic Cement
329 C1218/C1218M-99 Standard Test Method for Water-Soluble Chloride in Mortar and Concrete
332 C1240-05 Standard Specification for Silica Fume Used in Cementitious Mixtures
339 C1602/C1602M-06 Standard Specification for Mixing Water Used in the Production of Hydraulic Cement Concrete
343 C1609/C1609M-06 Standard Test Method for Flexural Performance of Fiber-Reinforced Concrete (Using Beam with Third-Point Loading)