ACI PRC-221-96: Guide for Use of Normal Weight and Heavyweight Aggregates in Concrete (Reapproved 2001) Topic: Aggregates Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 221 Published: 8/2002 Price:$ 57.50 USD Become a Member More Info »
ACI PRC-343-95: Analysis & Design of Reinforced Concrete Bridge Structures (Repproved 2004) Topic: Bridges Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 341 Published: 8/2002 Price:$ 160.50 USD Become a Member More Info »
ACI SPEC-336.1-01: Specification for the Construction of Drilled Piers Topic: Specifications Format: PDF Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 336 Published: 8/2002 Regular Price: $ 34.50 USD Member Price: $ 22.00 USD Become a Member More Info »
ACI PRC-357-84: Guide for the Design and Construction of Fixed Offshore Concrete Structures (Reapproved 1997) Topic: Marine Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 357 Published: 8/2002 Price:$ 54.50 USD Become a Member More Info »
ACI PRC-311.4-05: Guide for Concrete Inspection Topic: Inspection Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 311 Published: 10/2005 Price:$ 52.50 USD Become a Member More Info »
Slab Combination Pack Format: Protected PDF/Web View, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Published: 2/2007 Regular Price: $ 225.26 USD Member Price: $ 199.52 USD Become a Member More Info »
ACI PRC-440-07 Report on Fiber-Reinforced Polymer (FRP) Reinforcement for Concrete Structures Topic: Fiber-Reinforced Concrete Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 440 Published: 9/2007 Price:$ 99.50 USD Become a Member More Info »
ACI CODE-350M-06 Code Requirements for Environmental Engineering Concrete Structures & Commentary (Metric) Topic: Codes , Environmental Format: Protected PDF/Web View Unit: SI: International System of Units Language: English Author: ACI Committee 350 Published: 8/2008 Regular Price: $ 186.50 USD Member Price: $ 112.00 USD Become a Member More Info »
ACI PRC-550.1-09: Guide to Emulating Cast-in-Place Detailing for Seismic Design of Precast Concrete Structures (Reapproved 2017) Topic: Precast Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: Joint ACI/ASCE Committee 550 Published: 3/2009 Price:$ 53.50 USD Become a Member More Info »
ACI PRC-360-10 Guide to Design of Slabs-on-Ground Topic: Slabs Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 360 Published: 4/2010 Price:$ 105.00 USD Become a Member More Info »
ACI PRC-357.2-10 Report on Floating and Float-In Concrete Structures Topic: Marine Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 357 Published: 7/2010 Price:$ 76.50 USD Become a Member More Info »
ACI PRC-207.5-11 Report on Roller-Compacted Mass Concrete Topic: Mass Concrete Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 207 Published: 7/2011 Price:$ 101.50 USD Become a Member More Info »
ACI PRC-533-11 (Reapproved 2021) Guide for Precast Concrete Wall Panels Topic: Precast Concrete Format: PDF, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 533 Published: 2/2012 Price:$ 87.50 USD Become a Member More Info »
ACI PRC-303-12 Guide to Cast-in-Place Architectural Concrete Practice Topic: Architectural Concrete Format: PDF, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 303 Published: 6/2012 Price:$ 78.50 USD Become a Member More Info »
ACI PRC-308-213-13(22) Report on Internally Cured Concrete Using Prewetted Absorptive Lightweight Aggregate (Reapproved 2022) Topic: Curing Format: Protected PDF/Web View, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committees 308, 213 Published: 6/2013 Price:$ 56.50 USD Become a Member More Info »