Email Address is required Invalid Email Address
In todayโs market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have itโฆthey are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
Staff Directory
ACI World Headquarters 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA Phone: 1.248.848.3800 Fax: 1.248.848.3701
ACI Middle East Regional Office Second Floor, Office #207 The Offices 2 Building, One Central Dubai World Trade Center Complex Dubai, UAE Phone: +971.4.516.3208 & 3209
ACI Resource Center Southern California Midwest Mid Atlantic
Feedback via Email Phone: 1.248.848.3800
Home > Tools > Frequently Asked Questions
Q. Are epoxy resins widely used in concrete construction and repair? A. Epoxy resins are used with concrete in the form of coatings, repair materials, grouts, bonding agents, paints, adhesives, epoxy mortars, sealers, penetrating sealers, wearing surfaces, and as admixtures to hydraulic cement concrete to make epoxy polymer-modified concrete (ACI 503.7). References: SP-1(02); ACI 562-21; ACI 503.7; ACI 548.6R-19; ACI SPEC-548.9-21; ACI SPEC-548.13-21; ACI 548.14-14; ACI SPEC-548.15-20 Topics in Concrete: Epoxy in Concrete; Polymer Concrete; Repair of Concrete
Q. Are epoxy resins widely used in concrete construction and repair?
A. Epoxy resins are used with concrete in the form of coatings, repair materials, grouts, bonding agents, paints, adhesives, epoxy mortars, sealers, penetrating sealers, wearing surfaces, and as admixtures to hydraulic cement concrete to make epoxy polymer-modified concrete (ACI 503.7).
References: SP-1(02); ACI 562-21; ACI 503.7; ACI 548.6R-19; ACI SPEC-548.9-21; ACI SPEC-548.13-21; ACI 548.14-14; ACI SPEC-548.15-20
Topics in Concrete: Epoxy in Concrete; Polymer Concrete; Repair of Concrete